Root Cause Analysis of Surface Cracks in Heavy Steel Plates during the Hot Rolling Process
|
10.3390/met9070801
|
1398 - 04
|
|
Spark plasma sintering of Ni3Al-xB-1wt% CNT (0.0<x<1.5at%) nanocomposite
|
10.1016/j.jallcom.2019.02.225
|
1398 - 03
|
|
Microbiologically Influenced Corrosion of a Pipeline in a Petrochemical Plant
|
10.3390/met9040459
|
1398 - 01
|
|
Metallurgical aspects of a blowdown pipe failure in a petrochemical plant
|
10.1016/j.engfailanal.2019.01.068
|
1398 - 01
|
|
Spark plasma sintering of Stellite®-6 superalloy
|
10.1016/j.jallcom.2018.12.186
|
1398 - 01
|
|
Root Cause Analysis of Failure in Superheater Tubes in a Power Plant
|
10.1007/s13632-019-00533-4
|
1397 - 12
|
|
Modeling Electrical Resistivity of Naturally Aged Al-Mg-Si Alloys
|
10.3390/met9030310
|
1397 - 12
|
|
Microstructure and mechanical properties of spark plasma sintered nanocrystalline Ni3Al-xB (0.0<x<1.5 at%) alloy
|
10.1016/j.mtcomm.2018.09.002
|
1397 - 09
|
|
Influence of Ni/Co binders and Mo2C on the microstructure evolution and mechanical properties of (Ti0.93W0.07)C-based cermets
|
10.1016/j.ceramint.2018.06.227
|
1397 - 07
|
|
Failure of AISI 304H stainless steel elbows in a heat exchanger
|
10.1016/j.engfailanal.2018.04.006
|
1397 - 05
|
|
Metallurgical aspects of failure in a broken femoral HIP prosthesis
|
10.1016/j.engfailanal.2018.03.018
|
1396 - 12
|
|
The effects of boric acid on crystal structure, nano-/microstructure and photoluminescence characteristics of rare earth-doped Y2O3/YBO3 composite compounds
|
10.1007/s40097-017-0246-1
|
1396 - 08
|
|
The effects of boric acid on crystal structure nano/microstructure and photoluminescence characteristics of rare earth-doped Y2O3/YBO3 composite compounds
|
#
|
1396 - 08
|
|
Sigma phase-induced failure of AISI 310 stainless steel radiant tubes
|
10.1016/j.engfailanal.2017.08.027
|
1396 - 06
|
|
A case study on failure of AISI 347H stabilized stainless steel pipe in a petrochemical plant
|
#
|
1396 - 05
|
|
بررسي خواص و رفتار لا يه مياني Zr-%5.1Sn-Ti-Cu-Ag در اتصال غيرهمجنس آلومينا به مس
|
#
|
1404 - 01
|
|
ارزيابي اتصال غيرهمجنس آلومينا به مس با فلزپركننده فعال Sn-Ti-Cu-Ag و Zr-%3.5Sn-Ti-Cu-Ag به روش لحيم كاري سخت القايي
|
#
|
1403 - 01
|
|